不同发泡剂对锂渣泡沫玻璃显微结构和性能的影响

陈坤1, 廖其龙1, 刘来宝1, 王辅1, 竹含真1, 石贤盼1, 但勇2, 赵澎2   

  1. 1.西南科技大学材料与化学学院,绵阳 621010;
    2.四川顺应锂材料科技有限公司,眉山 620000
  • 收稿日期:2025-03-03 修订日期:2025-04-30 出版日期:2025-09-15 发布日期:2025-09-19
  • 通信作者: 廖其龙,博士,教授。E-mail:liaoqilong@swust.edu.cn
  • 作者简介:陈 坤(1998—),男。主要从事固废资源化利用研究。E-mail:792271744@qq.com
  • 基金资助:
    四川顺应锂材料科技有限公司资助项目(SYLK-JS-FW-2023-002)

Influences of Different Foaming Agents on Microstructure and Properties of Lithium Slag Foam Glass

CHEN Kun1, LIAO Qilong1, LIU Laibao1, WANG Fu1, ZHU Hanzhen1, SHI Xianpan1, DAN Yong2, ZHAO Peng2   

  1. 1. School of Materials and Chemistry, Southwest University of Science and Technology, Mianyang 621010, China;
    2. Sichuan Shunying Lithium Material Technology Co., Ltd., Meishan 620000, China
  • Received:2025-03-03 Revised:2025-04-30 Published:2025-09-15 Online:2025-09-19

摘要: 随着锂电池产业的快速发展,巨量锂渣的资源化利用成为当前亟待解决的问题。本研究以锂渣为主要原料,分别引入MnO2、SiC和CaCO3作为发泡剂,制备泡沫玻璃,系统探究了不同发泡剂种类及掺量对泡沫玻璃发泡过程、孔结构与物理性能的影响,并揭示了相应的发泡机制。结果表明:MnO2和CaCO3掺量增加导致孔径增大,体积密度、抗压强度和导热系数减小;SiC掺量增加则使孔径减小,体积密度、抗压强度和导热系数增大。过量的MnO2形成开孔结构,SiC和CaCO3则形成闭孔结构。当MnO2掺量为4%~5%(质量分数)和SiC掺量为1%~2%(质量分数)时,泡沫玻璃综合性能最优,体积密度介于0.35~0.44 g/cm3,抗压强度为1.24~2.99 MPa,导热系数为0.058~0.065 W/(m·K),满足行业标准。本研究为锂渣的高值化利用提供了理论支撑和技术路径。

关键词: 锂渣, 泡沫玻璃, 发泡剂, 孔结构, 物理性能, 发泡机理

Abstract: With the rapid development of the lithium battery industry, the resource utilization of the massive amount of lithium slag has become an urgent issue to be solved. In this study, lithium slag was used as the main raw material to prepare foam glass, with MnO2, SiC and CaCO3 introduced as foaming agents. The effects of different types and content of foaming agents on the foaming process, pore structure and physical properties of the foam glass were systematically investigated, and the corresponding foaming mechanisms were elucidated. The results show that increase the content of MnO2 and CaCO3 leads to increase of pore size and decrease of bulk density, compressive strength and thermal conductivity. With the increase of SiC content, pore size decreases and bulk density, compressive strength and thermal conductivity increase. Excessive MnO2 forms open-cell structures, whereas SiC and CaCO3 forms closed-cell structures. When the MnO2 content is 4%~5% (mass fracton) and SiC content is 1%~2% (mass fracton), the foam glass exhibits optimal comprehensive performance, with a bulk density of 0.35~0.44 g/cm3, compressive strength of 1.24~2.99 MPa, and thermal conductivity of 0.058~0.065 W/(m·K), meeting industry standard. This study provides theoretical support and a technical pathway for the high-value utilization of lithium slag.

Key words: lithium slag, foam glass, foaming agent, pore structure, physical property, foaming mechanism

中图分类号: