BULLETIN OF THE CHINESE CERAMIC SOCIETY ›› 2022, Vol. 41 ›› Issue (8): 2918-2926.
• Glass • Previous Articles Next Articles
ZHENG Jiexi1, GONG Kuiyuan2, ZHANG Hongyang3, XUE Hongxi1, XU Kunshan1, LIU Jie1
Received:
2022-02-16
Revised:
2022-05-23
Online:
2022-08-15
Published:
2022-08-30
CLC Number:
ZHENG Jiexi, GONG Kuiyuan, ZHANG Hongyang, XUE Hongxi, XU Kunshan, LIU Jie. Action Mechanism and Research Progress of Flux and Adhesive on Glass Lining[J]. BULLETIN OF THE CHINESE CERAMIC SOCIETY, 2022, 41(8): 2918-2926.
[1] LIAO Y M, ZHANG B, CHEN M H, et al. Self-healing metal-enamel composite coating and its protection for TiAl alloy against oxidation under thermal shock in NaCl solution[J]. Corrosion Science, 2020, 167: 108526. [2] ROSSI S, CALOVI M, VELEZ D, et al. Influence of addition of hard particles on the mechanical and chemical behavior of vitreous enamel[J]. Surface and Coatings Technology, 2019, 357: 69-77. [3] 陈 肯.BTC1钢表面搪瓷涂层的密着和耐硫酸露点腐蚀机制研究[D].合肥:中国科学技术大学,2019:7-10. CHEN K. Study on the adhesion and sulfuric acid dew point corrosion resistance of enamel coating on BTC1 steel[D]. Hefei: University of Science and Technology of China, 2019: 7-10 (in Chinese). [4] 邵规贤,芶文彬,闻瑞昌,等.搪瓷学[M].北京:轻工业出版社,1983:55-59. SHAO G X, GOU W B, WEN R C, et al. Enamel[M]. Beijing: China Light Industry Press, 1983: 55-59 (in Chinese). [5] 卢进标.中国搪瓷手册[M].北京:中国轻工业出版社,2001:122-140. LU J B. China enamel manual[M]. Beijing: China Light Industry Press, 2001: 122-140 (in Chinese). [6] GIN S, JOLLIVET P, FOURNIER M, et al. Origin and consequences of silicate glass passivation by surface layers[J]. Nature Communications, 2015, 6: 6360. [7] CHEN K, CHEN M H, YU Z D, et al. Simulating sulfuric acid dew point corrosion of enamels with different contents of silica[J]. Corrosion Science, 2017, 127: 201-212. [8] 银 怀,黎红英,陈基东,等.磷酸盐涂层研究进展及其应用[J].表面技术,2021,50(1):232-241. YIN H, LI H Y, CHEN J D, et al. Research progress and application of phosphate coatings[J]. Surface Technology, 2021, 50(1): 232-241 (in Chinese). [9] 张定军,鲜彦博,马彦军,等.无机磷酸盐基复合涂层在表面防护技术中的研究现状及应用进展[J].表面技术,2020,49(7):68-75. ZHANG D J, XIAN Y B, MA Y J, et al. Research progress of inorganic phosphate-based composite coatings in the surface protection fields[J]. Surface Technology, 2020, 49(7): 68-75 (in Chinese). [10] CAI L X, LI Y, WANG S S, et al. Investigation of the erosion damage mechanism and erosion prediction of boronized coatings at elevated temperatures[J]. Materials (Basel, Switzerland), 2020, 14(1): 123. [11] PANDA J N, WONG B C, MEDVEDOVSKI E, et al. Enhancement of tribo-corrosion performance of carbon steel through boronizing and BN-based coatings[J]. Tribology International, 2021, 153: 106666. [12] CHEN K, CHEN M H, YU Z D, et al. Corrosion of SiO2-B2O3-Al2O3-CaF2-R2O (R=Na and K) enamels with different content of ZrO2 in H2SO4 and NaOH solutions[J]. Ceramics International, 2019, 45(12): 14958-14967. [13] 唐 旋,马 倩,王 俊,等.ZrO2含量对工业搪瓷瓷层化学稳定性及结构的影响[J].硅酸盐通报,2018,37(9):2979-2984. TANG X, MA Q, WANG J, et al. Effect of ZrO2 content on chemical stability and structure of industrial enamel[J]. Bulletin of the Chinese Ceramic Society, 2018, 37(9): 2979-2984 (in Chinese). [14] 吴静沛.碳钢表面低温搪瓷涂层的制备及性能研究[D].杭州:浙江工业大学,2014:8-9. WU J P. The preparation of low firing enamel coating on carbon steel and its performance[D]. Hangzhou: Zhejiang University of Technology, 2014: 8-9 (in Chinese). [15] 赵彦钊,王一迪,胡智敏,等.低温无铅乳浊玻璃釉性能研究[J].陕西科技大学学报(自然科学版),2015,33(1):46-50+56. ZHAO Y Z, WANG Y D, HU Z M, et al. Performance investigation of lead-free opaque glass glaze at lower temperature[J]. Journal of Shaanxi University of Science and Technology (Natural Science Edition), 2015, 33(1): 46-50+56 (in Chinese). [16] KUMAR K R, PRIDHAR T, SREE B V S. Mechanical properties and characterization of zirconium oxide (ZrO2) and coconut shell ash(CSA) reinforced aluminium (Al 6082) matrix hybrid composite[J]. Journal of Alloys and Compounds, 2018, 765: 171-179. [17] KO H, LEE S J, OH J J, et al. Physiochemical effects of SiC and ZrO2 particle fillers on the properties of enamel coatings[J]. Coatings, 2020, 10(2): 121. [18] WANG S H, LI X N, WANG Y Q, et al. Corrosion resistance and clean ability of glazed surface[J]. International Journal of Applied Ceramic Technology, 2020, 17(5): 2162-2170. [19] FENG D D, ZHU Y M, LI F F, et al. Influence investigation of CaF2 on the LAS based glass-ceramics and the glass-ceramic/diamond composites[J]. Journal of the European Ceramic Society, 2016, 36(10): 2579-2585. [20] 薛洪喜,崔永凤,徐坤山,等.搪玻璃使用寿命及其理化性能研究进展[J].硅酸盐通报,2020,39(12):3991-3997. XUE H X, CUI Y F, XU K S, et al. Research progress on service life and physicochemical properties of enamel[J]. Bulletin of the Chinese Ceramic Society, 2020, 39(12): 3991-3997 (in Chinese). [21] PRADELL T, MOLINA G, MOLERA J, et al. The use of micro-XRD for the study of glaze color decorations[J]. Applied Physics A, 2013, 111(1): 121-127. [22] 关宝强,牛占堂,刘 云,等.墙地砖生产釉浆流速性能及常用添加剂研究[J].佛山陶瓷,2018,28(9):20-23+27. GUAN B Q, NIU Z T, LIU Y, et al. Glaze slurry performance of velocity of flow and common additives in wall and floor tiles production[J]. Foshan Ceramics, 2018, 28(9): 20-23+27 (in Chinese). [23] ROSSI S, CALOVI M, VELEZ D, et al. Microstructural analysis and surface modification of a vitreous enamel modified with corundum particles[J]. Advanced Engineering Materials, 2019, 21(8): 1900231. [24] 张进超.高硬度耐高温腐蚀搪瓷层制备工艺研究[D].大连:大连交通大学,2007:4. ZHANG J C. Process of high-hardness and high-temperature erosion resistance enamel on steel[D]. Dalian: Dalian Jiaotong University, 2007: 4 (in Chinese). [25] 王衍行,祖成奎,陈 江.组成对高硼硅玻璃粘度和膨胀系数的影响[J].功能材料,2012,43(21):2985-2988. WANG Y H, ZU C K, CHEN J. Effect of components on viscosities and coefficients of thermal expansion of borosilicate glasses[J]. Journal of Functional Materials, 2012, 43(21): 2985-2988 (in Chinese). [26] 唐 旋,马 倩,张兆明,等.Li2O质量分数对工业搪瓷耐酸性能的影响[J].东华大学学报(自然科学版),2019,45(3):396-400. TANG X, MA Q, ZHANG Z M, et al. Effect of Li2O mass fraction on acid resistance of industrial enamel[J]. Journal of Donghua University (Natural Science), 2019, 45(3): 396-400 (in Chinese). [27] 周新艳,程金树,康俊峰,等.碱金属氧化物对CaO-MgO-Al2O3-SiO2玻璃黏度和析晶性能的影响[J].武汉理工大学学报,2015,37(3):8-12. ZHOU X Y, CHENG J S, KANG J F, et al. Effect of alkali mental oxides on viscosity and crystallization behavior of Ca O-MgO-Al2O3-SiO2 glass-ceramics[J]. Journal of Wuhan University of Technology, 2015, 37(3): 8-12 (in Chinese). [28] 周 琦,王枫成,南雪丽,等.碱金属氧化物对镍渣微晶玻璃性能的影响[J].兰州理工大学学报,2010,36(6):17-20. ZHOU Q, WANG F C, NAN X L, et al. Influence of alkali metal oxides on property of glass-ceramic with nickel slag[J]. Journal of Lanzhou University of Technology, 2010, 36(6): 17-20 (in Chinese). [29] 徐建华,邱永斌,张留生,等.陶瓷花釉与装饰技术[M].北京:中国轻工业出版社,2011:17. XU J H, QIU Y B, ZHANG L S, et al. Ceramic glaze and decoration technology[M]. Beijing: China Light Industry Press, 2011: 17 (in Chinese). [30] ZHOU M K, GE X X, WANG H D, et al. Effect of the CaO content and decomposition of calcium-containing minerals on properties and microstructure of ceramic foams from fly ash[J]. Ceramics International, 2017, 43(12): 9451-9457. [31] XI X A, XU L F, SHUI A Z, et al. Effect of silicon carbide particle size and CaO content on foaming properties during firing and microstructure of porcelain ceramics[J]. Ceramics International, 2014, 40(8): 12931-12938. [32] 张 彬,王 静,汤何锐,等.碱土金属氧化物对无碱硼铝硅酸盐玻璃性能的影响[J].材料科学与工程学报,2018,36(5):824-828. ZHANG B, WANG J, TANG H R, et al. Effect of alkaline earth metal oxide on physicochemical properties of alkali-free boron aluminum silicate glasses[J]. Journal of Materials Science and Engineering, 2018, 36(5): 824-828 (in Chinese). [33] GE X X, ZHOU M K, WANG H D, et al. Effects of flux components on the properties and pore structure of ceramic foams produced from coal bottom ash[J]. Ceramics International, 2019, 45(9): 12528-12534. [34] 方久华,杨 峰,左明扬,等.玻璃配合料中铬渣最大允许用量研究[J].无机盐工业,2015,47(1):18-21. FANG J H, YANG F, ZUO M Y, et al. Research on the biggest allowable level of chrome residue in mixed batch of glass[J]. Inorganic Chemicals Industry, 2015, 47(1): 18-21 (in Chinese). [35] BELTRAN M, BROCK F, PRADELL T. Thermal properties and stability of Catalan Modernist blue and green enamels[J]. International Journal of Applied Glass Science, 2019, 10(3): 414-425. [36] JIN M, XU J Y, SHI M L, et al. Growth of high performance piezoelectric crystal Pb(Zn1/3Nb2/3)O3-PbTiO3 using PbO flux[J]. Ultrasonics, 2007, 46(2): 129-132. [37] 戴长禄,杨 勇,杨 明.锌在建筑陶瓷坯体、釉料及微晶玻璃中的作用与影响[J].佛山陶瓷,2012(4):29-32. DAI C L, YANG Y, YANG M. Effect and influence of zinc in building ceramic bodies, glaze and microcrystalline glass[J]. Foshan Ceramics, 2012(4): 29-32 (in Chinese). [38] 王 超,杨 茵.碱土金属氧化物对硼熔块釉的影响分析[J].人工晶体学报,2018,47(10):2212-2215+2222. WANG C, YANG Y. Influence of alkaline-earth metallic oxide on boron fritted glaze quality[J]. Journal of Synthetic Crystals, 2018, 47(10): 2212-2215+2222 (in Chinese). [39] 张临安.高温熔块釉的制备与性能研究[D].大连:大连工业大学,2015:5-6. ZHANG L A. The preparation and performance analysis of high temperature frit glaze[D]. Dalian: Dalian Polytechnic University, 2015: 5-6 (in Chinese). [40] 徐开东,王继娜,李志新,等.基于赤泥和硅灰的泡沫玻璃制备及性能研究[J].硅酸盐通报,2019,38(12):3897-3904. XU K D, WANG J N, LI Z X, et al. Preparation and properties of foam glass based on red mud and silica fume[J]. Bulletin of the Chinese Ceramic Society, 2019, 38(12): 3897-3904 (in Chinese). [41] 安科云,尹荔松,阳素玉,等.Na2B4O7在降低釉料烧成温度中的作用[J].中国陶瓷,2010,46(1):53-56+63. AN K Y, YIN L S, YANG S Y, et al. The effects of Na2B4O7 on reducing the melting temperature of glaze[J]. China Ceramics, 2010, 46(1): 53-56+63 (in Chinese). [42] 朱仁萍,徐光青,吴玉程,等.硼砂对粉煤灰多孔玻璃结构及性能的影响[J].硅酸盐通报,2011,30(1):177-181. ZHU R P, XU G Q, WU Y C, et al. Influence of borax on the structure and properties of porous glass[J]. Bulletin of the Chinese Ceramic Society, 2011, 30(1): 177-181 (in Chinese). [43] KOUDELKA L, MONER P. Borophosphate glasses of the ZnO-B2O3-P2O5 system[J]. Materials Letters, 2000, 42(3): 194-199. [44] QU L, ZHANG X Q, DUAN H Y, et al. The application of LIBS and other techniques on Chinese low temperature glaze[J]. MRS Advances, 2017, 2(39/40): 2081-2094. [45] XU K S, XUE H X, ZHENG J X, et al. Improving the mechanical impact and bending resistances of enamel via B2O3 addition[J]. Ceramics International, 2021, 47(19): 27195-27200. [46] ANDREOLA F, BARBIERI L, CORRADI A, et al. CRT glass state of the art[J]. Journal of the European Ceramic Society, 2007, 27(2/3): 1623-1629. [47] MAYYAS M, PAHLEVANI F, HANDOKO W, et al. Preliminary investigation on the thermal conversion of automotive shredder residue into value-added products: graphitic carbon and nano-ceramics[J]. Waste Management, 2016, 50: 173-183. [48] ZHOU X H, LI X Y, YANG F, et al. Study on the physics and dielectric property of Al2O3-B2O3-SiO2/Al2O3 glass+ceramic[J]. Journal of Materials Science: Materials in Electronics, 2016, 27(12): 12654-12659. [49] ZHERNOVAYA N F, BURCHAKOVA Y V, ZHERNOVOI F E, et al. Low-melting non-frit glazes for construction and artistic ceramics[J]. Glass and Ceramics, 2013, 70(3/4): 104-106. [50] ADEDIRAN A, LEMOUGNA P N, YLINIEMI J, et al. Recycling glass wool as a fluxing agent in the production of clay- and waste-based ceramics[J]. Journal of Cleaner Production, 2021, 289: 125673. [51] 蒲永平,殷立雄,刘 陈,等.低氟搪瓷钛面釉的研制[J].西北轻工业学院学报,2001,19(1):26-29. PU Y P, YIN L X, LIU C, et al. Development of low-fluorine titanium coat enamel[J]. Journal of Northwest Institute of Light Industry, 2001, 19(1): 26-29 (in Chinese). [52] 涂 欣,王 晴.硼硅酸盐泡沫玻璃复合材料的研制[J].新型建筑材料,2013,40(7):36-39. TU X, WANG Q. Research on the preparation of borosilicate foam glass[J]. New Building Materials, 2013, 40(7): 36-39 (in Chinese). [53] YU Z D, CHEN M H, CHEN K, et al. Corrosion of enamel with and without CaF2 in molten aluminum at 750 ℃[J]. Corrosion Science, 2019, 148: 228-236. [54] ZUCCHELLI A, DIGNATICI M, MONTORSI M, et al. Characterization of vitreous enamel-steel interface by using hot stage ESEM and nano-indentation techniques[J]. Journal of the European Ceramic Society, 2012, 32(10): 2243-2251. [55] BUKOVEC M, XHANARI K, LEER T, et al. Analysis of the enameled AISI 316LVM stainless steel[J]. Journal of Materials Engineering and Performance, 2018, 27(3): 1122-1129. [56] CHA J, SHIN J, BAE J, et al. Compositional dependence of structure and wetting properties of CoO-doped silicate glass for porcelain enamel[J]. Journal of the Ceramic Society of Japan, 2018, 126(6): 469-474. [57] CHEN K, CHEN M H, YU Z D, et al. Exploring the hindering mechanism of element Ti on the adherence of CoO-bearing one-coat enamel/steel[J]. International Journal of Applied Ceramic Technology, 2019, 16(1): 185-194. [58] 唐景平,蒋伟忠.氧化镍在搪瓷密着及抑制鳞爆中的作用[J].中国搪瓷,2003,24(s2):22-27+49. TANG J P, JIANG W Z. The role of nickel oxide in enamel and inhibiting scales[J]. China Enamel, 2003, 24(s2): 22-27+49 (in Chinese). [59] CHA J, KIM J, SHIN J, et al. Effect of nano-NiO additive on adhesion strength and bubble structure of vitreous enamels[J]. Journal of the Korean Physical Society, 2018, 72(7): 770-774. [60] 叶佳意,钱蕙春,蒋伟忠,等.超细镍酸锂晶体对搪瓷密着强度影响的研究[J].玻璃与搪瓷,2008,36(4):5-8+12. YE J Y, QIAN H C, JIANG W Z, et al. Study on influence of mill addition of super fine Li2Ni8O10 crystals on enamel adherent strength[J]. Glass & Enamel, 2008, 36(4): 5-8+12 (in Chinese). [61] TANG F J, CHENG X M, CHEN G D, et al. Electrochemical behavior of enamel-coated carbon steel in simulated concrete pore water solution with various chloride concentrations[J]. Electrochimica Acta, 2013, 92: 36-46. [62] 廖依敏,陈明辉,王福会,等.自修复金属搪瓷高温防护涂层[J].表面技术,2020,49(1):25-34. LIAO Y M, CHEN M H, WANG F H, et al. Self-healing high-temperature protective metal-enamel composite coatings[J]. Surface Technology, 2020, 49(1): 25-34 (in Chinese). [63] CHEN K, CHEN M H, WANG Q C, et al. Micro-alloys precipitation in NiO- and CoO-bearing enamel coatings and their effect on adherence of enamel/steel[J]. International Journal of Applied Glass Science, 2018, 9(1): 70-84. [64] 张大明.含钡低温底釉对钢板的密着性[J].硅酸盐通报,1984,3(3):24-28. ZHANG D M. The adhesion to steel sheets containing rhetor-containing low temperature under glaze[J]. Bulletin of the Chinese Ceramic Society, 1984, 3(3): 24-28 (in Chinese). [65] BRANZEI M, PENCEA I, MATEI A A, et al. Influence of high temperature exposure on the adhesion of a micro-composite refractory enamel to a Ni-18Cr-12W superalloy[J]. Journal of Adhesion Science and Technology, 2017, 31(23): 2555-2570. [66] 王海燕,程 麟,凌志达.搪瓷瓷釉与金属之间的密着[J].玻璃与搪瓷,2007,35(5):33-35+42. WANG H Y, CHENG L, LING Z D. Adherence mechanisms between enamel and metal[J]. Glass & Enamel, 2007, 35(5): 33-35+42 (in Chinese). [67] LING G P, HE J H. The influence of nano-Al2O3 additive on the adhesion between enamel and steel substrate[J]. Materials Science and Engineering: A, 2004, 379(1/2): 432-436. [68] 舒明勇,尹海英,刘光辉,等.选钛尾矿制备钒钛搪瓷及性能研究[J].表面技术,2016,45(10):13-19. SHU M Y, YIN H Y, LIU G H, et al. Preparation and properties of V-Ti enamel by ilmenite tailings[J]. Surface Technology, 2016, 45(10): 13-19 (in Chinese). [69] SHU M Y, YIN H Y, ZHONG Q D, et al. Effect of glass powder on acid resistance of enamel coating[J]. Surface Review and Letters, 2017, 24(3): 1750036. |
[1] | ZHANG Yue, WANG Hongjie, YANG Lin, CHEN Hong, CAO Jianxin. Influence of Phosphogypsum Particle Size on Properties and Microstructure of Wet-Mixed Mortar [J]. BULLETIN OF THE CHINESE CERAMIC SOCIETY, 2022, 41(8): 2836-2843. |
[2] | KONG Yaning, ZHOU Jianwei, GAO Yuxin, YANG Wen, YU Baoying, CHENG Baojun. Sodium Sulfate Corrosion Resistance of Gypsum Slag Cement Concrete [J]. BULLETIN OF THE CHINESE CERAMIC SOCIETY, 2022, 41(8): 2844-2850. |
[3] | WANG Xin, WEI Ming, LIU Kun. Research Progress on Control and Preparation of Vaterite-Type Calcium Carbonate [J]. BULLETIN OF THE CHINESE CERAMIC SOCIETY, 2022, 41(8): 2860-2870. |
[4] | QUAN Zhilin, LI Zhixiang, JIAO Bin, ZHOU Xianwei, XIANG Dexing, FENG Xiaoqin, HUANG Hongsheng. Preparation of KBaB5O9 by Two-Step Method and Its Process Kinetics [J]. BULLETIN OF THE CHINESE CERAMIC SOCIETY, 2022, 41(8): 2954-2962. |
[5] | CHEN Yu, LI Chuangchuang, LI Guohao, DONG Kai, LIU Ronggui, LU Chunhua. Chloride Penetration Resistance of Cement Mortar Modified by Graphene Oxide [J]. BULLETIN OF THE CHINESE CERAMIC SOCIETY, 2022, 41(5): 1539-1546. |
[6] | WEI Kang, LI Ben, SUN Qiao. Improving Chloride Ion Penetration Resistance of Recycled Concrete by Basalt Fiber [J]. BULLETIN OF THE CHINESE CERAMIC SOCIETY, 2022, 41(5): 1656-1662. |
[7] | WANG Min, LI Yawei, YAN Shuang. Preparation and Compressive Strength of Geopolymer Cementitious Material Based on High Temperature Activated Molybdenum Tailings [J]. BULLETIN OF THE CHINESE CERAMIC SOCIETY, 2022, 41(5): 1689-1695. |
[8] | GE Menglong, YE Qianqian, KANG Haijiao, LI Jianzhang. Research Progress of Admixture-Modified Magnesium Oxychloride Cement [J]. BULLETIN OF THE CHINESE CERAMIC SOCIETY, 2022, 41(4): 1202-1210. |
[9] | BO Ai, ZHANG Dajiang, WANG Huangqi, WANG Dongmin, WANG Qibao, LIU Ze. Influence of Calcination Process on C2S Crystal Transformation in Natural Hydraulic Lime [J]. BULLETIN OF THE CHINESE CERAMIC SOCIETY, 2022, 41(4): 1336-1342. |
[10] | MA Xiaoyu, WANG Hongjun, WEI Hong. Effects of Different Heating Treatment Temperatures on Composition and Structure of BiMnO3 Nanoparticles [J]. BULLETIN OF THE CHINESE CERAMIC SOCIETY, 2022, 41(4): 1473-1478. |
[11] | WU Jianfeng, WU Changhu, XU Xiaohong, TIAN Kezhong, LIU Yang, MA Sitong. Preparation of Ceramic Facing Brick from Gold Tailings [J]. BULLETIN OF THE CHINESE CERAMIC SOCIETY, 2022, 41(2): 640-648. |
[12] | CHEN Gaixia, YIN Yanping, LUO Yaofei. Effect of Basalt Fiber on Performance ofSteel Slag-Asphalt Mixture [J]. BULLETIN OF THE CHINESE CERAMIC SOCIETY, 2022, 41(2): 657-666. |
[13] | SHI Magang, KE Guojun, ZOU Pinyu, SONG Baixing, TANG Xiaolin, JIN Dan. Research Progress of Hydration, Mechanical and Dry Shrinkage Properties of Alkali-Activated Slag Cement [J]. BULLETIN OF THE CHINESE CERAMIC SOCIETY, 2022, 41(1): 162-173. |
[14] | LI Jing, LIU Jinkun, YAN Tingting, LENG Chongyan, CHEN Xiliang, CHEN Qinghua. Research Progress on Preparation of Magnetic Hydroxyapatite [J]. BULLETIN OF THE CHINESE CERAMIC SOCIETY, 2022, 41(1): 302-311. |
[15] | CAO Tianyi, XIA Guanghua, CHENG Yue, LI Senlin. Basic Properties and Application Evaluation of Clay in Rongchang Area [J]. BULLETIN OF THE CHINESE CERAMIC SOCIETY, 2021, 40(9): 3122-3129. |
Viewed | ||||||
Full text |
|
|||||
Abstract |
|
|||||