BULLETIN OF THE CHINESE CERAMIC SOCIETY ›› 2008, Vol. 27 ›› Issue (1): 142-146.

Previous Articles     Next Articles

Preparation of Mesoporous Titanium Dioxide Using a Composite Surfactant Template and Super-Critical Desiccation Technique

WU Xiao-xia;ZHOU Da-li;LU Yun;OU Yuz-hi;YANG Weizhong;DENG Yin-deng;CHEN Yan-wen   