欢迎访问《硅酸盐通报》官方网站,今天是
分享到:

硅酸盐通报 ›› 2021, Vol. 40 ›› Issue (3): 723-730.

• 水泥混凝土 • 上一篇    下一篇

超轻硫铝酸盐水泥基发泡材料的制备及硬化性能研究

王上1, 刘松辉1, 周蓉1, 张跃宏1, 张海波1,2   

  1. 1.河南理工大学材料科学与工程学院,焦作 454003;
    2.河南省深地材料科学与技术重点实验室,焦作 454003
  • 收稿日期:2020-10-29 修回日期:2020-12-08 出版日期:2021-03-15 发布日期:2021-04-13
  • 通讯作者: 张海波,博士,副教授。E-mail:zzhb@hpu.edu.cn
  • 作者简介:王 上(1995—),男,硕士研究生。主要从事绿色建筑材料方面的研究。E-mail:648665647@qq.com
  • 基金资助:
    国家重点研发计划(2017YFC0603004);河南省自然科学基金(182300410207)

Preparation and Hardening Performance of Ultra-Light Sulphoaluminate Cement-Based Foaming Material

WANG Shang1, LIU Songhui1, ZHOU Rong1, ZHANG Yuehong1, ZHANG Haibo1,2   

  1. 1. School of Materials Science and Engineering, Henan Polytechnic University, Jiaozuo 454003, China;
    2. Henan Key Laboratory of Materials on Deep-Earth Engineering, Jiaozuo 454003, China
  • Received:2020-10-29 Revised:2020-12-08 Online:2021-03-15 Published:2021-04-13

摘要: 针对传统硅酸盐水泥基发泡材料膨胀倍率小、容重与干密度较大、凝结时间长等问题,采用硫铝酸盐水泥熟料、石灰和硬石膏作为胶凝材料,双氧水(H2O2)为发泡剂,羟丙基甲基纤维素醚(HPMC)为稳泡剂制备了超轻硫铝酸盐水泥基发泡材料(U-SCFM),系统研究了H2O2用量、HPMC掺量及水胶比对U-SCFM膨胀倍率、干密度及硬化强度等性能的影响规律,并通过超景深显微镜、热分析(TGA)、扫描电子显微镜(SEM)等对U-SCFM硬化体的水化产物及微观结构进行表征。结果表明:当水胶比为0.8,H2O2和HPMC掺量分别为胶凝材料质量的10%和1%时,制备出膨胀倍率为4.2、干密度为265 kg/m3、7 d抗压强度达到0.98 MPa的U-SCFM材料;HPMC的增稠作用及U-SCFM快速凝结硬化形成钙矾石晶体是U-SCFM硬化体多孔结构形成的主要原因。以上结果为煤矿巷道高冒区的充填提供了一种绿色安全、低成本充填材料。

关键词: 硫铝酸盐水泥熟料, 充填材料, 发泡, 稳泡, 双氧水

Abstract: Aiming at the problems of traditional Portland cement-based foaming materials, such as small expansion ratio, large bulk density and dry density, and long setting time. An ultra-light sulfoaluminate cement-based foaming material (U-SCFM) was prepared using sulfoaluminate cement clinker, lime and hard gypsum as cementitious materials, hydrogen peroxide (H2O2) as blowing agent and hydroxypropyl methylcellulose ether (HPMC) as foam stabilizer.The influence of H2O2 dosage, HPMC content and water-binder ratio on the expansion ratio, dry density, and hardening strength of U-SCFM were systematically researched. The hydration products and microstructure of U-SCFM hardened body were also characterized by using the ultra-depth-of-field microscope, thermal analysis (TGA), scanning electron microscope (SEM). The results show that when the water-binder ratio is 0.8, H2O2 and HPMC content are respectively 10% and 1% of the cementitious materials mass, U-SCFM with an expansion ratio of 4.2, dry density of 265 kg/m3, and 7 d compressive strength of 0.98 MPa is prepared. The thickening effect of HPMC and the rapid setting and hardening of U-SCFM to form ettringite crystals are the main reasons for the formation of the porous structure of the U-SCFM hardened body. The above results provide a green, safe, low-cost filling material for filling the high-collapse area of coal mine tunnels.

Key words: sulphoaluminate cement clinker, filling material, foaming, foam stabilizer, hydrogen peroxide

中图分类号: