[1] 姚 燕,王发洲,余其俊,等.海洋工程高抗蚀水泥基材料研究进展[J].中国基础科学,2019,21(3):1-10+16. YAO Y, WANG F Z, YU Q J, et al. Progress of study on cement-based materials with high erosion resistance for marine engineering[J]. China Basic Science, 2019, 21(3): 1-10+16 (in Chinese). [2] ZHANG K C, SHEN P L, YANG L, et al. Development of high-ferrite cement: toward green cement production[J]. Journal of Cleaner Production, 2021, 327: 129487. [3] 高金瑞,饶美娟,张克昌,等.铁相组分对铁相和高铁低钙水泥熟料水化性能及抗侵蚀性能影响[J].硅酸盐通报,2021,40(4):1097-1102+1115. GAO J R, RAO M J, ZHANG K C, et al. Effect of iron phase component on hydration performance and corrosion resistance of iron phase and high-iron low-calcium cement clinker[J]. Bulletin of the Chinese Ceramic Society, 2021, 40(4): 1097-1102+1115 (in Chinese). [4] 朱 明,曾 浪,饶美娟.高铁低钙硅酸盐水泥体系的抗氯离子侵蚀性能研究[J].硅酸盐通报,2018,37(10):3136-3140. ZHU M, ZENG L, RAO M J. Resistance to chloride ion erosion of high-iron low-calcium silicate cement[J]. Bulletin of the Chinese Ceramic Society, 2018, 37(10): 3136-3140 (in Chinese). [5] KJELLSEN K O, DETWILER R J. Reaction kinetics of Portland cement mortars hydrated at different temperatures[J]. Cement and Concrete Research, 1992, 22(1): 112-120. [6] LIN F, MEYER C. Hydration kinetics modeling of Portland cement considering the effects of curing temperature and applied pressure[J]. Cement and Concrete Research, 2009, 39(4): 255-265. [7] ESCALANTE-GARCÍA J I, SHARP J H. The microstructure and mechanical properties of blended cements hydrated at various temperatures[J]. Cement and Concrete Research, 2001, 31(5): 695-702. [8] THOMAS J J, JENNINGS H. Effect of heat treatment on the pore structure and drying shrinkage behavior of hydrated cement paste[J]. Journal of the American Ceramic Society, 2002, 85: 2293-2298. [9] REINHARDT H W, STEGMAIER M. Influence of heat curing on the pore structure and compressive strength of self-compacting concrete (SCC)[J]. Cement and Concrete Research, 2006, 36(5): 879-885. [10] KIM J K, HAN S H, SONG Y C. Effect of temperature and aging on the mechanical properties of concrete: part I. experimental results[J]. Cement and Concrete Research, 2002, 32(7): 1087-1094. [11] 何 伟,周予启.早期高温养护对混凝土后期宏观性能的影响[J].混凝土,2018(10):47-51. HE W, ZHOU Y Q. Effect of early high temperature curing on the late-age performance of concrete[J]. Concrete, 2018(10): 47-51 (in Chinese). [12] 魏玲玲,贺智敏,李一鸣,等.矿物掺合料对蒸养混凝土传输性能和孔结构的影响[J].水资源与水工程学报,2020,31(1):179-186. WEI L L, HE Z M, LI Y M, et al. Influence of mineral admixtures on transportation properties and pore structure of steam-cured concrete[J]. Journal of Water Resources and Water Engineering, 2020, 31(1): 179-186 (in Chinese). [13] 张文华,张云升.高温养护条件下现代混凝土水化、硬化及微结构形成机理研究进展[J].硅酸盐通报,2015,34(1):149-155. ZHANG W H, ZHANG Y S. Research progress on the hydration, hardening and microstructure formation mechanism of modern concrete under high temperature curing conditions[J]. Bulletin of the Chinese Ceramic Society, 2015, 34(1): 149-155 (in Chinese). [14] 熊蓉蓉,龙广成,宋军伟.蒸养条件下掺矿物掺合料水泥复合浆体的水化特性研究[J].硅酸盐通报,2018,37(11):3630-3636. XIONG R R, LONG G C, SONG J W. Study of mineral admixtures on the hydration characteristic of complex binder under steam curing condition[J]. Bulletin of the Chinese Ceramic Society, 2018, 37(11): 3630-3636 (in Chinese). [15] 黄 啸.高铁低钙硅酸盐海工水泥及其混凝土制品性能研究[D].武汉:武汉理工大学,2019. HUANG X. The performance high ferrite low alite Portland marine cement and its concrete products[D]. Wuhan: Wuhan University of Technology, 2019 (in Chinese). [16] TANG L P, NILSSON L O. Chloride binding capacity and binding isotherms of OPC pastes and mortars[J]. Cement and Concrete Research, 1993, 23(2): 247-253. [17] CHEN X F, HE Y J, LU L N, et al. Effects of curing regimes on the chloride binding capacity of cementitious materials[J]. Construction and Building Materials, 2022, 342: 127929. [18] BARNETT S J, SOUTSOS M N, MILLARD S G, et al. Strength development of mortars containing ground granulated blast-furnace slag: effect of curing temperature and determination of apparent activation energies[J]. Cement and Concrete Research, 2006, 36(3): 434-440. [19] MA Y F, LI W W, JIN M, et al. Influences of leaching on the composition, structure and morphology of calcium silicate hydrate (C-S-H) with different Ca/Si ratios[J]. Journal of Building Engineering, 2022, 58: 105017. [20] 刘 世,刘海卿,王锦力.煤矸石掺量对混凝土毛细吸水特性影响的试验研究[J].硅酸盐通报,2017,36(12):4313-4318. LIU S, LIU H Q, WANG J L. Experimental study on effects of the contents of coal gangue aggregates on the water absorption capacity of concrete[J]. Bulletin of the Chinese Ceramic Society, 2017, 36(12): 4313-4318 (in Chinese). [21] MEHTA P K, MONTEIRO P. Concrete: microstructure, properties, and material[M].3rd ed. New York: McGraw-Hill, 2006. [22] 王小东,张启志,曹中顺.复掺粉煤灰和超细矿渣对高性能混凝土力学与耐久性能的影响研究[J].当代化工,2022,51(1):35-38. WANG X D, ZHANG Q Z, CAO Z S. Study on the influence of mixing fly ash and superfine slag on the mechanics and durability of high performance concrete[J]. Contemporary Chemical Industry, 2022, 51(1): 35-38 (in Chinese). [23] HUANG X, HU S G, WANG F Z, et al. The effect of supplementary cementitious materials on the permeability of chloride in steam cured high-ferrite Portland cement concrete[J]. Construction and Building Materials, 2019, 197: 99-106. |